Bio TyphimuriumBiofilm Sidewall StrontiuTitanate SKKU NUS Calcium MagneticForceMicroscopy contact Blend Ananth Sperm Lattice Battery Ni81Fe19 Pattern Neodymium CrossSection Croatia CrystalGrowing suspended_graphene ScanningTunnelingMicroscopy DNAProtein Non-ContactMode HighResolution LeakageCurrent alkanes Ucl Electronics YttriaStabilizedZirconia PetruPoni_Institute Mosfet Optoelectronic pinpoint mode TCS
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Star of Graphene
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 0.6 Hz
- Scan Size : 2.5μm×2.5μm
- Pixel Size : 256×256
- Cantilever : Multi75-G (k=3N/m, f=75kHz)