FuelCell University_of_Regensburg DiffractiveOpticalElements thermal_conductivity blended polymers SiliconeOxide Ca10(PO4)6(OH)2 Cancer Granada fifber Forevision Blend nanomechanical Indium_tin_oxide exfoliate SetpointMode Graphite LightEmiting TipBiasMode food Tungsten Self-assembledMonolayer Permalloy amplitude_modulation CuParticle StrontiuTitanate MfmAmplitude FrequencyModulation LowDensityPolyethylene pinpoint mode MagneticArray STM PolycrystallineFerroelectricBCZT ThermalProperties Copolymer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polycrystalline ferroelectric BCZT
Scanning Conditions
- System: NX12
- Scan Mode: PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.4Hz
- Pixel: 256×256
- Sample bias sweep range for Piezoresponse curve: -10V ~ +10V