Transparent Chungnam_National_University Piezo PiezoelectricForceMicroscopy Tin disulfide semifluorinated alkane Singapore Molybdenum Treatment 2-vinylpyridine nanobar ForceVolumeImage SiWafer Tapping Electrical&Electronics PS_PVAC Litho Friction self-assembly Force-distance Silicon Cell LiquidCell Electical&Electronics CuSubstrate DeoxyribonucleicAcid Sic Ucl HumanHair Moire HexacontaneFilm ContactMode Piezoresponse ThermalProperties NTU
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Trench Etch Profile on MESA
Top dielectric trench etch profile on MESA on Si wafer.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 6μm×6μm
- Scan Rate: 0.12Hz
- Pixel Size: 1024 × 256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 6μm×6μm
- Scan Rate: 0.12Hz
- Pixel Size: 1024 × 256