Electrode Metal-organicComplex SrTiO3 Yttria_stabilized_Zirconia Ceramic dichalcogenide MagneticForceMicroscopy GaN Genetic Temperature Biology Global_Comm hydrocarbon Ceramics LateralPFM Zagreb FM-KPFM mono_layer Laser Thermal SicMosfet PpLdpe ScanningIon-ConductanceMicroscopy Nanotechnology Plug PolycrystallineFerroelectricBCZT PatternedSapphireSubstrat Co/Cr/Pt MfmPhase Insulator FrictionForce HOPG ScanningSpreadingResistanceMicroscopy GaAs Hexatriacontane
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256